E295 — unalloyed machine structural steel. Rm 460-580 MPa as rolled. For shafts, axles, bolts and general engineering components requiring higher strength than S275 without alloying.
E295 per EN 10025-2 (1.0533). Designation E (engineering) vs S (structural) indicates tighter dimensional tolerances and surface quality for machined parts. Carbon typically 0.25-0.35% gives Rm 460-580 MPa in hot-rolled bar without heat treatment. Used for shafts, axles, couplings, bolts and general engineering machined components requiring moderate strength.